Author | Message |
---|---|
OHCRJ79![]() Members ![]() ![]() ![]() ![]() Add As Buddy Posts: 36
Location: Kentucky
Occupation: Airline pilot but playing aircraft dispatcher right now
Age:
|
Post #77611, posted on 02-14-2021 GMT-5 hours
|
And this is what happens. I sprayed it, let it dry for an hour and used sanding pads starting at 3600 grit all the way up to 12000 and then sprayed again. I repeated this step 3 times. What it's done it created a shine that I've never gotten out of a metalizer and the sanding has harden the paint. It doesnt lift with tape and finger prints can be wiped away with a damp cloth. |
Author | Message |
---|---|
skyking918![]() Upper Deck Member ![]() ![]() ![]() ![]() Add As Buddy Posts: 723
Location: Carrollton, TX
Occupation: Aviation historian/writer (freelance)
Age: 74
|
|
Too bad it’s been discontinued.
Michael McMurtrey |